Menu
F
As extruded only.
T1
Solution treated and quenched from an elevated temperature as part of the extrusion process and naturally aged.
T4
Solution treated and quenched from an elevated temperature as part of the extrusion process and naturally aged. Applies to products that are not cold worked, or where the effect of cold work is not recognised in applicable standards.
T5
Solution treated, cooled from an elevated temperature as part of the extrusion process and then artificially aged to substantially improve mechanical properties.
T52
A temper satisfying T5 requirements with improved formability.
T6
Solution treated, cooled from an elevated temperature as part of the extrusion process and then artificially aged to give maximum mechanical properties.
Note: A second or third digit maybe added to designated tempers. This indicates a variation in the production process has been applied to alter the final characteristic of the product, i.e. to achieve improved ductility etc